The infrared transmittance of a high-optical-quality chemical vapor deposition (CVD) diamond sample was independently measured by The Johns Hopkins University Applied Physics Laboratory, Rockwell International, and Texas Instruments, Inc., from room temperature to 780 K.At0.75 mm thick, the sample is one of the thickest high-optical-quality CVD diamond samples produced so far. Measurements were taken with both dual-beam grating spectrometers and a Fourier transform spectrometer so that experimental artifacts of a particular instrument could be identified and reduced. The data sets were in good agreement from room temperature to 780 K. This work definitively establishes the high-temperature optical properties of CVD diamond.
© (1994) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Michael E. Thomas and Alan B. Harker "Temperature dependence of absorption in CVD diamond", Proc. SPIE 2286, Window and Dome Technologies and Materials IV, (28 September 1994); https://doi.org/10.1117/12.187376
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Diamond

Chemical vapor deposition

Temperature metrology

Spectrometers

Transmittance

Absorption

Mass attenuation coefficient

RELATED CONTENT

Continuum water vapor absorption in the 4000 8000 cm 1...
Proceedings of SPIE (November 19 2015)
Optical properties of diamond
Proceedings of SPIE (September 28 1994)
Scattering and absorption of CVD diamond windows
Proceedings of SPIE (December 14 1992)
Multiphonon difference band absorption in diamond
Proceedings of SPIE (May 20 2011)

Back to Top